S275JR

Data verified

S275JR is the middle step of the EN 10025-2 structural family, offering about 17% more yield strength than S235JR at a small price premium. It is a common choice where S235 is marginally too weak but S355 is not needed.

DIN1.0044 (S275JR)
AISIA572 Gr.42 (near)
JISSS490 (near)
CategoryStructural & HSLA Steel

Chemical composition

ElementContent (%)
C≤0.21
Mn≤1.50
P≤0.035
S≤0.035
Cu≤0.55

Weight percent, per the governing standard ranges. Actual values per heat are on the mill certificate.

Properties

Yield strength≥275 MPa (≤16 mm)
Tensile strength410–560 MPa
ImpactJR: 27 J at 20 °C
Density7.85 g/cm³

Heat treatment

Supplied hot rolled; no hardening treatment.

Equivalent grades

StandardDesignation
din1.0044 (S275JR)
aisiA572 Gr.42 (near)
jisSS490 (near)
gbQ275 (legacy, near)

Equivalents overlap in chemistry and use but are not always identical — see our equivalents guide before substituting in certified designs.

Applications & Processing

Applications: Bridges, crane girders, machinery frames, medium-duty construction.

Processing: Very good weldability; carbon equivalent stays low enough for standard procedures without preheat in thin and medium plate.

Need S275JR from stock?

Steel.Wiki is sponsored by Shenzhen NewAsia Special Steel (Nasteel), a special-steel stockholder in Shenzhen stocking mold, tool and alloy steels with EN 10204 3.1 certification.

Ask for a quotationVisit Nasteel

Source: EN 10025-2 published ranges · Last updated 2026-11-03. Data is indicative — verify critical values against the governing standard and mill certificate before use.