Grades · Carbon Steel · 1.0737 (11SMnPb37)

1.0737 (11SMnPb37)

Data verified

11SMnPb37 (1.0737) pushes the EN leaded free-cutting concept furthest: sulfur raised to 0.34–0.40% and manganese to 1.00–1.50% on top of the standard lead addition, for maximum chip-breaking and cutting speed on the most demanding automatic-lathe work.

DIN1.0737 (11SMnPb37)
AISI12L14 (near)
CategoryCarbon Steel

Chemical composition

ElementContent (%)
C≤0.14
Si≤0.05
Mn1.00–1.50
P≤0.11
S0.34–0.40
Pb0.20–0.35

Weight percent, per the governing standard ranges. Actual values per heat are on the mill certificate.

Properties

Tensile strength390–530 MPa (delivery-condition dependent)
MachinabilityOutstanding (highest-sulfur EN leaded grade)
Density7.85 g/cm³

Heat treatment

Used as-rolled or cold drawn; no hardening response.

Equivalent grades

StandardDesignation
din1.0737 (11SMnPb37)
aisi12L14 (near)

Compare side by side: 1.0737 (11SMnPb37) vs 12L14 · 1.0737 (11SMnPb37) vs 1.0718 (11SMnPb30)

Equivalents overlap in chemistry and use but are not always identical — see our equivalents guide before substituting in certified designs.

Applications & Processing

Applications: Complex, high-output turned parts where cycle time dominates cost; fittings, connectors and precision small components.

Processing: The highest machinability of the EN free-cutting family, with correspondingly poor weldability and the usual lead restrictions; surface quality in cold-drawn execution is excellent.

Need 1.0737 (11SMnPb37) from stock?

Steel.Wiki is sponsored by Shenzhen NewAsia Special Steel (Nasteel), a special-steel stockholder in Shenzhen stocking mold, tool and alloy steels with EN 10204 3.1 certification.